CONTROL FO FLOW OGSOL(Osaka Gas Chemical)
Characteristics
- High refractive index, High heat resistance, Low shrinkage, High Flexibility
 
                                 Physical property data  
                            
| Acrylate monomer | Mixture | ||||
|---|---|---|---|---|---|
| Product name | OGSOL EA-0200 | OGSOL EA-0300 |  【Development】 OGSOL GA-5000  | 
                                        OGSOL EA-F5710 | |
| Feature |  High refractive index High heat resistance  | 
                                         High Flexibility High heat resistance  | 
                                         Ultra-high refractive index  | 
                                         High refractive index Solvent-Free  | 
                                    |
|  Before Curing  | 
                                        Refractive index | 1.616 | 1.555 | 1.620 | 1.601 | 
| Color(APHA) | Approx, 5% toluene | NO | 30%MIBK | NO | |
| Solvent presence | >100,000 | 6,000-8,000 | 8,000-12,000 | 8,000-12,000 | |
|  Viscosity [mPa・s](25°C)  | 
                                        <100 | <100 | <500 | <100 | |
|  After Curing  | 
                                        Refractive index | 1.626 | 1.576 | 1.650 | 1.623 | 
| Tg(DSC)[°C] | 211 | 17 | 228 | 127 | |
|  Volume shrinkage [%]  | 
                                        0.5 | NO DATA | NO DATA | NO DATA | |
|  Water absorption [%]  | 
                                        0.08 | 2.60 | NO DATA | NO DATA | |
                                * There is the 50% PGMEA dilution OGSOL EA-0200 (Product name: OGSOL EA-0250P) 
                                  Curing Condition
                                  Photo iniciator : 3phr Irgacure 184 
                                  Irradiation device : High -pressure mercury lamp 
                                  Integrated UV light intencity : 360 mJ/cm2 
                            
Thermal yellowing test
| Product name | OGSOL EA-0200 | OGSOL EA-0300 | OGSOL GA-5000【Development】 | |||
|---|---|---|---|---|---|---|
| Test condition | Before the test | 230 ℃ × 30 분 | Before the test | 230 ℃ × 30 분 | Before the test | 230 ℃ × 30 분 | 
| Appearance |     | 
                                            | 
                                            | 
                                    |||
| transmittance[%] | 99.4 | 97.9 | 99.6 | 97.9 | 99.7 | 95.8 | 